Chromic anhydride (CrO3) thermal decomposition method: the chromic anhydride is heated to 13,000 tons at 900 ° C under high temperature conditions. It is a metallurgical grade oxidative decomposition prepared by reduction of sodium chromate in the Tiejin gold plant. Get the finished product. In recent years, the chromium oxide produced by this method in China has developed extremely violently. In 1999, the production of chromium oxide by chromic anhydride was about twice that of chromium.
The thermal decomposition process of chromic anhydride is complicated, and with the increase of temperature, chromic anhydride will be decomposed into four kinds of chromium oxides.
Since chromic anhydride melts at about 200 ° C and begins to decompose, and oxygen and chromium oxide are precipitated, the chromium oxide crystals gradually form and grow in the chromic anhydride melt as the temperature increases. This method has a large number of crystal defects, can maintain many excellent properties of chrome oxide single crystal, and has high product quality, so it is widely used.
Studies have shown that Cr2O3 is present when the temperature rises to 470 °C. It has been completely converted to Cr2O3 at 550V. However, during the test, it was found that the actual decomposition temperature was higher than this temperature. The reason is Cr2O3. During the decomposition process, Cr2O3 is generated. The film is coated on the surface of the unconverted chromium oxide, while Cr2O3. The melting point is very high (2266 ± 25) ° C, and the heat transfer is poor, hindering the further decomposition of chromium oxide. To this end, a process of adding a small amount of water can be employed to lower the reaction temperature. On the one hand CrO3. Very soluble in water, on the other hand can make additives with CrO3. The quality score has reached more than 99%.
The reaction temperature and time also have a great influence on the decomposition of chromic anhydride. In general, the higher the temperature, the shorter the reaction time. A series of experiments with temperature-independent reactions and TEM photographs at this temperature show that it is difficult to completely convert chromic anhydride to Cr2O3 below 650 °C. The sample contains a large amount of needle-like crystals containing a large amount of needle-like crystals (CrO2). As the temperature increases, the particles gradually become larger, and there is a significant sintering phenomenon at 900 °C.